Overview

THIN SET mortar, a polymer-modified Portland Cement blend featuring graded aggregates and specialized additives, is formulated to provide an advanced setting mortar. Ideal for all types of ceramic, quarry tiles, marble, pavers, and natural stone for both floor and wall installations, it surpasses ANSI A 118.4 standards when mixed with water. This premium, preblended thin set mortar is tailor-made for bonding masonry thin veneer units, including both manufactured and natural thin stone, as well as thin brick to substrates in both indoor and outdoor settings. Its cutting-edge anti-sag properties and precise sand gradation ensure outstanding workability, adhesion, and longevity, making it essential for masonry applications.

Shear Bond Strength (ANSI A 118.4)
Glazed Wall Tile (Vitreous Tile)
28 days................................................ 800 psi
Impervious Ceramic Tile Mortar Tile (Non-Vitreous Tile)
28 days................................................ 450 psi
Quarry Tile
28 days................................................ 500 psi
Shear Bond Strength to Plywood (ASTM C-882)
28 days............................................... 200 psi
Compressive Strength (ASTM C- 109)
28 days............................................ 3,600 psi
TCA Service Rating (ASTM C-627) Extra Heavy
Set Time (ASTM C-266)
Initial ……………………………………. 4 hours
Final ………………………………….…. 7 hours
Open Time at 72 ……………….. 15-20 minutes
Pot Life at 72 ……………………...…. 3-4 hours

THIN SET exceeds ANSI 118.4 when mixed with water.

LIMITATIONS:

Do not apply over frozen or frost laden substrates. Temperature must remain above 45

for a minimum of 72 hours after application.